Abstract of the Disclosure There is disclosed a lithium aluminosilicate glass body encased within, and integral with, a thin, compressive, semicrystalline layer containing beta-eucryptite and/or beta-quartz solid solution crystals, and a method of producing such body. The layer has a substantially lower thermal coefficient of expansion than the glass, but has the same chemical composition as the glass. That composition, in percent by weight on a calculated oxide basis is 55-67% SiO2, 5.0-7.5% Li20, 22-28% A1203, 0-2% Na2O and 0-10% ZnO, the molar ratio of R20+R0 to A1203 being greater than one. Controlled crystallization procedure is described whereby the crystallized layer can be produced in a relatively short time.
558441
Beall George H.
Pierson Joseph E.
Stookey Stanley D.
Corning Incorporated
Gowling Lafleur Henderson Llp
LandOfFree
Strengthened glass article and method does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Strengthened glass article and method, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Strengthened glass article and method will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1335872