Disclosed is a method of making an optical fiber preform having at least one annular region of depressed refractive index. A tube of silica doped with fluorine and/or boron is overclad with silica soot. A core rod is inserted into the overclad tube and the resultant assembly is heated while chlorine flows between the tube and the core rod to clean the adjacent surfaces. When the soot consolidates, the tube collapses onto and fuses to the rod. The resultant tubular structure is provided with cladding and drawn to form an optical fiber which exhibits low attenuation as a result of the low seed count at the interface between the inner core and the region that is doped with florine and/or boron.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of making optical fiber having depressed index core... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making optical fiber having depressed index core..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making optical fiber having depressed index core... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2060813

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.