Abstract New alloys used as a raw material for preparing apertured rotatory cylinder applied in manufacturing glass fibers using high speed centrifugal force ejection. This alloy consists essentially of 0.08 to 0.8% of C, 15 to 35% of Cr, 1.3 to 5.4% of W, 0.1 to 0.26% of Ti, 0.12 to 0.25% of Zr and 1% Nb and the remainder constituted by Ni and impurities unavoidably carried into the alloy.

416458

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Alloy resistant to corrosion and wear at elevated temperature does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Alloy resistant to corrosion and wear at elevated temperature, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Alloy resistant to corrosion and wear at elevated temperature will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1323161

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.