ABSTRACT An alumina-zirconia composite sintered product which comprises a zirconia crystalline phase composed mainly of a tetragonal zirconia and an alumina crystalline phase is described. The sintered product has such a fine structure that regions of said alumina crystalline phase being separated with the zirconia crystalline phase at a size of from 0.1 to 2 µm on average. Preferably, the zirconia crystalline phase contains not larger than 4 mol% of yttrium oxide or not larger than 14 mol% of cerium oxide as a stabilizer. A method for making a starting composite powder and a method for making a composite sintered product using the composite powder are also described.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Alumina-zirconia composite sintered product and method for... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Alumina-zirconia composite sintered product and method for..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Alumina-zirconia composite sintered product and method for... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1729307

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.