Impact modified styrenic polymers with improved stress crack...

C - Chemistry – Metallurgy – 08 – L

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C08L 25/00 (2006.01) C08J 3/20 (2006.01) C08L 23/00 (2006.01) C08L 23/22 (2006.01)

Patent

CA 2754923

A method of improving the stress crack resistance of an impact modified styrenic polymer comprising (a) combining about 95 to about 99.5 wt.% of an impact modified styrenic polymer with about 0.5 to about 5 wt.% of a polymer solution comprising about 25 to about 75 wt.% polyisobutylene and about 25 to about 75 wt.% of a polyolefin comprising one or more C2 to C12 alpha olefins.

La présente invention concerne un procédé d'amélioration de la résistance à la rupture sous contrainte d'un polymère de styrène anti-chocs comprenant l'étape consistant à : (a) combiner environ 95 à environ 99,5 % en poids d'un polymère de styrène anti-chocs avec environ 0,5 à environ 5 % en poids d'une solution de polymère comprenant environ 25 à environ 75 % en poids de polyisobutylène et environ 25 à environ 75 % en poids d'une polyoléfine comprenant une ou plusieurs alpha-oléfines en C2 à C12.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Impact modified styrenic polymers with improved stress crack... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Impact modified styrenic polymers with improved stress crack..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Impact modified styrenic polymers with improved stress crack... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1442666

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.