C - Chemistry – Metallurgy – 09 – C
Patent
C - Chemistry, Metallurgy
09
C
6/210
C09C 1/42 (2006.01) C09C 1/00 (2006.01) D21H 17/67 (2006.01) D21H 17/68 (2006.01) D21H 19/40 (2006.01) D21H 17/69 (2006.01)
Patent
CA 1253659
ABSTRACT OF THE DISCLOSURE A substantially white, anhydrous, amorphous alumino- silicate pigment is obtained by calcining a combination of previously uncalcined kaolin clay and an alumina source. The calcination is carried out at a temperature of about 870°C to 1400°C, preferably about 870°C to 1260°C, for a suitable period of time, e.g., 0.1 to 3 hours. The pigments obtained by the foregoing method display enhanced brightness greater than the merely additive brightness which would be obtained by mixing alumina with a previously calcined kaolin clay and are otherwise well suited for use as paper-filling or coating pigments.
498845
Catone David L.
Huege Fred R.
Slepetys Richard A.
Engelhard Corporation
Sim & Mcburney
LandOfFree
Kaolin clay-based pigment does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Kaolin clay-based pigment, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Kaolin clay-based pigment will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1322864