C - Chemistry – Metallurgy – 03 – B
Patent
C - Chemistry, Metallurgy
03
B
49/45
C03B 27/04 (2006.01) C03B 27/044 (2006.01)
Patent
CA 1191691
Abstract Federal Specification DD-G-1403B requires heat-strengthened glass to have a surface compression stress not less than 3500 pounds per square inch nor greater than 10,000 pounds per square inch and an edge compression stress that is not less than 5500 pounds per square inch. Large windows conforming to this specification are believed to have little likelihood to develop dangerous islands of glass that separate from the glass sheets when they fracture. The present invention provides method and apparatus to develop heat-strengthened glass sheets of large dimensions such as used for commercial construction that develop suitable break patterns when fractured.
416605
Gowling Lafleur Henderson Llp
Ppg Industries Ohio Inc.
LandOfFree
Method and apparatus for producing heat-strengthened glass... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method and apparatus for producing heat-strengthened glass..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method and apparatus for producing heat-strengthened glass... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1246537