A method for flexibilizing a glass fiber nonwoven bound with a cured urea formaldehyde resin binder by admixing water, a cured urea formaldehyde resin, and a water-soluble polymer comprising a polymerized ethylenically unsaturated carboxylic acid monomer, the polymer having a weight average molecular weight of from about 65,000 to about 95,000; applying the aqueous admixture to a glass fiber nonwoven; and heating the admixture to at least about 120°C. Also disclosed are glass fiber nonwovens made using the method.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for flexibilizing glass fiber nonwoven bound with... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for flexibilizing glass fiber nonwoven bound with..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for flexibilizing glass fiber nonwoven bound with... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2031998

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.