C22C 38/28 (2006.01) B21B 17/14 (2006.01) B21B 47/02 (2006.01) B21C 37/08 (2006.01) C22C 38/04 (2006.01) C22C 38/06 (2006.01) C22C 38/18 (2006.01) C22C 38/22 (2006.01) C22C 38/26 (2006.01) C22C 38/58 (2006.01)
Patent
CA 2550680
A method is provided for manufacturing a high-strength, as-welded steel pipe product, with a minimum yield strength in excess of 80 ksi (552 MPa), suitable for use in oil and gas well casings, without the need for a post-weld heat treatment which would otherwise be required to obtain an as-welded pipe having that level of strength.
Hansen Steven S.
Russo Joseph D.
Heenan Blaikie Llp
Ipsco Enterprises Inc.
LandOfFree
Method for making high-strength steel pipe, and pipe made by... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for making high-strength steel pipe, and pipe made by..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for making high-strength steel pipe, and pipe made by... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1485300