Method for preparing modified wooden material

B - Operations – Transporting – 27 – K

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

B27K 3/34 (2006.01) B27K 3/00 (2006.01) B27K 3/36 (2006.01) C09K 3/18 (2006.01)

Patent

CA 2392656

Wooden materials are advantageously modified with the treatment of the product of co-hydrolytic condensation of (A) 100 parts by weight of an organosilicon compound having the formula: (R1)a(OR2)b SiO(4-a-b)/2(1) wherein R1 is alkyl, R2 is alkyl, 0.75 <= a <= 1.5, 0.2 <= b <= 3 and 0.9 < a+b <= 4, and (B) 0.5-49 parts by weight of an amino-containing alkoxysilane having the formula: R3R4NR5-SiR6n (OR2)3-n (2) wherein R3 and R4 are H or alkyl or aminoalkyl, R5 is a divalent hydrocarbon group, R6 is alkyl, and n is 0 or 1, or a partial hydrolyzate thereof in the presence of an organic acid or inorganic acid.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method for preparing modified wooden material does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for preparing modified wooden material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for preparing modified wooden material will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1732505

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.