A method of providing a tin oxide coating on a moving flat or float glass substrate by chemical vapour deposition by pre-mixing gaseous streams of tin tetrachloride and water at a temperature of between 100°C and 240°C and directing the unitary pre-mixed stream against the glass in substantially laminar flow, the tin tetrachloride and the water only reacting in the region of the surface of the glass to form the tin oxide coating on the glass. Alternatively, gaseous streams of anhydrous hydrogen chloride, tin tetrachloride and water may be premixed to form the unitary pre-mixed stream, which pre-mixed stream impacts the glass in substantially laminar flow, the tin tetrachloride and the water reacting with one another in the region of the glass to form tin oxide which forms a coating on the glass.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of coating glass does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of coating glass, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of coating glass will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1382926

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.