Method of increasing the dynamical strength of glass container

C - Chemistry – Metallurgy – 03 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

204/91.47

C03C 17/34 (2006.01) B01J 19/12 (2006.01) C03C 17/32 (2006.01)

Patent

CA 1333785

A method of increasing the pressure-resistant strength and impact strength of a glass container, which comprises treating the surface of the glass container with a silane coupling agent, applying a coating material comprising a reactive compound having at least two (meth)acryloyl groups in the molecule to the treated glass container, and subjecting it to irradiation of an activated energy ray to cure the coating material applied; and a method of increasing the pressure- resistant strength and impact strength of a glass con- tainer, which comprises applying a coating material comprising a silane coupling agent and a reactive com- pound having at least two (meth)acryloyl groups in the molecule to the surface of the glass article, and then subjecting the coated glass container to irradiation of an activated energy ray to cure the coating.

565209

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of increasing the dynamical strength of glass container does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of increasing the dynamical strength of glass container, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing the dynamical strength of glass container will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1292891

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.