Method of making polarization retaining fiber

C - Chemistry – Metallurgy – 03 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C03B 37/027 (2006.01) C03B 37/012 (2006.01) C03B 37/014 (2006.01) C03C 15/00 (2006.01) C03C 25/68 (2006.01)

Patent

CA 2054873

Disclosed is a method of making a polarization retaining single-mode optical fiber. Longitudinal grooves are formed on opposite sides of a cylindrically-shaped core preform having a glass core surrounded by cladding glass. The core preform is inserted into a glass tube, the tube is shrunk onto the core preform, and the interface between the core preform and the tube is fused to form a solid preform having longitudinal apertures on opposite sides of the core. An etchant gas is flowed through the apertures to enlarge the apertures into holes having a substantially round cross-section. Inserted into each aperture is a stress rod formed of glass having a coefficient of expansion different from that of the cladding glass. The resultant draw blank is drawn to form a single-mode optical fiber having a core that is subjected to a stress-induced birefringence.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of making polarization retaining fiber does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making polarization retaining fiber, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making polarization retaining fiber will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1923508

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.