A method for mitigating stress corrosion cracking of a component exposed to a high temperature water (68) in a high temperature water system is provided. The method (68) comprises the steps of lowering corrosion potential conditions to a desired low corrosion potential (70) in the high temperature water environment; and introducing a first material comprising zinc (72) into the high temperature water environment, such that the desired low corrosion potential facilitates transport of the first material into cracks in a structure communicative with the high temperature water environment.
Andresen Peter Louis
Angeliu Thomas Martin
Diaz Thomas Pompilio
Hettiarachchi Sam
Kim Young-Jin
Company General Electric
Craig Wilson And Company
LandOfFree
Mitigation of stress corrosion cracking of structural... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Mitigation of stress corrosion cracking of structural..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Mitigation of stress corrosion cracking of structural... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1654295