C - Chemistry – Metallurgy – 22 – C
Patent
C - Chemistry, Metallurgy
22
C
C22C 19/05 (2006.01) F01D 5/28 (2006.01)
Patent
CA 2711325
A nickel-based superalloy particularly suitable for the fabrication of mechanical components for a piece of turbomachinery characterized in that it comprises at least the following elements in percentage by weight: chromium between 3% and 7%; tungsten between 3% and 15%; tantalum between 4% and 6%; aluminium between 4% and 8%; carbon less than 0.8%; the remaining percentage of nickel plus impurities.
Carosi Andrea
Giambi Barbara
Innocenti Marco
Maresca Pasquale
Tassa Oriana
Craig Wilson And Company
Nuovo Pignone S.p.a.
LandOfFree
Nickel-based superalloy, mechanical component made of the... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-based superalloy, mechanical component made of the..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-based superalloy, mechanical component made of the... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1908048