6/206, 117/47.7

C09C 3/08 (2006.01) C09D 17/00 (2006.01) D21H 17/67 (2006.01)

Patent

CA 2010869

A titanium dioxide pigment slurry containing from about 70 to about 80 percent by weight solids content is provided by dewatering, at superatmospheric pressure, a highly dispersed pigment slurry containing from about 20 to about 50 percent by weight of an untreated, nonflocculated titanium dioxide pigment and which slurry has a pH of below about 4.0 or above about 8.0 to produce a wet filter cake. The wet filter cake is reslurried in the presence of a dispersing agent. The high solids content slurry preferably is prepared from rutile titanium dioxide pigment.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing high solids slurries does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing high solids slurries, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing high solids slurries will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1596612

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.