ABSTRACT A process for producing a propylene block copolymer by a three-step reaction in the presence of a stereoregular catalyst. At the first step, propylene is polymerized at a temperature of 55°C or more to form polypropylene having an intrinsic viscosity of from 0.5 to 3.5 in the prescribed amount. At the second step, propylene is polymerized at a temperature of from 30 to 90°C to form polypropylene having an intrinsic viscosity of at least 4 in the prescribed amount. And at the third step, ethylene and propylene are copolymerized at a temperature of from 30 to 90°C to form an ethylene- propylene copolymer having an intrinsic viscosity of at least three in the prescribed amount. The propylene block copolymer formed by the three steps is superior and well balanced in impact resistance and stiffness.
443200
Kasahara Toshikazu
Nishikawa Tsutomu
Idemitsu Petrochemical Company Limited
Riches Mckenzie & Herbert Llp
LandOfFree
Process for the production of propylene block copolymers does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for the production of propylene block copolymers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of propylene block copolymers will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1194937